Figure 2
A sequence of q-scans of the 113 Bragg reflection during (a) slow cooling from 140 K (HS-R3 phase) to 118 K (LS-dis phase) and (b) subsequent heating to 139 K (HS-R3 phase). The corresponding changes of (c) peak positions and (d) peak intensities.  [article HTML]