[Figure 3]
Figure 3
(a) Evolution of the volume fraction for the indicated heating rates during continuous heating experiments on the Al-Zn-Mg alloy, initially in the TGP state. (b) Reversion during 10 K min-1 heating of three initial states, TGP, T[eta]' and T[eta] (Deschamps, Genevois et al., 2005BB12; courtesy Taylor & Francis).