Figure 1
Pole figures measured for the 111, 200 and 220 reflections of a nickel film deposited at 2 A dm-2 with an additive concentration of 5 mMol dm-3. The iso-intensity lines in the contour plots correspond to pole density levels drawn from 1 to 3 in steps of 0.25. As for all other films, the rotational symmetry in the pole figures indicates the presence of ideal fiber textures.  [article HTML]