Figure 7
Grain growth in Al–0.1%Mn. Shown are the maps for the first four layers in the initial state (above) and the corresponding maps for the same layers after heating (below). The fully reconstructed grain volumes – covering 40 layers – comprised 491 and 49 grains, respectively. The colour scale is related to the crystallographic orientation of the individual grain. From Schmidt et al. (2008). |