Figure 8
(a) Bright-field transmission electron microscopy and (b) high-resolution transmission electron microscopy images of the alloy annealed at 1123 K for 30 min, quenched to room temperature, annealed at 823 K for 30 min, and finally quenched to room temperature. The diameter of the spherical precipitates is approximately 5 nm.  [article HTML]