Figure 7
Comparison of the 00-032-1586 and 00-036-1639 XRD patterns (CCD PDF2) with the patterns simulated for the modelled, 1M, 2M, 3M, 4M and 5M, and the experimental, 6M, polytypes. The wavelength 1.540 Å (Cu) was used for the simulation.  [article HTML]