Figure 14
Data from cement after being sprayed with water, taken at 1 min intervals. This gives an indication of the change in lattice parameters during hydration and recovery after dehydration. The upper profile is the projection of the intensity from 15-40 min after dehydration. The sample was rocked during data collection and the start of data collection was ~10 s after spraying.  [article HTML]