(a), (b) Fe(110) diffraction intensity after (a) 0 and (b) 140 min of corrosion of mild steel in CO2-saturated 0.5 M NaCl solution at 353 K under potentiostatic control [−500 mV versus Ag/AgCl/KCl (saturated)]. (c), (d) Plots from which the fractal dimension D can be extracted, for (c) 0 and (d) 140 min.