Figure 1
Scattered intensity of NaCp* at T = 295 K as a function of the diffraction angle [2\theta]. Shown are the observed pattern ([\diamond]), the best fit profile in Cmcm (a), the difference curve between observed and calculated profiles (b) and the reflection markers (vertical bars). The wavelength is [\lambda] = 0.491213 (2) Å. The higher-angle part starting at 13° [2\theta] is enlarged by a factor of 10.