view article

Figure 3
X-ray powder pattern of hemihydrate (CaSO4·0.5H2O) at 300 K and 30% relative air humidity with tungsten (W) as an internal standard [observed pattern (circles), the best LeBail fit profiles (line), and the difference curve between the observed and the calculated profiles (below)].