X-ray powder pattern of the subhydrate (CaSO4·0.625H2O) at 300 K and 75% relative air humidity with tungsten (W) as an internal standard [observed pattern (circles), the best LeBail fit profiles (line), and the difference curve between the observed and the calculated profiles (below)].