Figure 6
Temperature dependence of the unit-cell parameters a and c of SBN with an Sr content of 0.822 (black dots with error bars). For lower temperatures, the results taken from Quadri et al. (2005 ) were plotted (squares) and converted to different compositions (0.75 versus 0.822). The gray arrows denote the piezoelectric contributions to the thermal expansion (see text). |


journal menu![[Figure 6]](ws5047fig6.jpg)