Figure 2
Li2WO4 crystals grown by the LTG Cz technique at different crystallization rates: (a) crystallization rate 1.5 mm h−1, rotation rate 5 rpm; (b) crystallization rate 0.5 mm h−1, rotation rate 5 rpm. |
|
|
|
Figure 2
Li2WO4 crystals grown by the LTG Cz technique at different crystallization rates: (a) crystallization rate 1.5 mm h−1, rotation rate 5 rpm; (b) crystallization rate 0.5 mm h−1, rotation rate 5 rpm. |