Figure 3
Li2WO4 crystals grown by the LTG Cz technique at different rotation rates and varying controlled temperature gradients between three heating zones: (a) crystallization rate of 0.5 mm h−1, rotation rate 10 rpm; (b) crystallization rate of 0.5 mm h−1, rotation rate 5 rpm |