Figure 4
Molybdenum-doped Li2W1–xMoxO4 crystals (x = 0.0125, 0.05) grown using the LTG Cz technique: (a) Li2W0.9875Mo0.0125O4 (1.25 mol% Mo); (b) Li2W0.95Mo0.05O4 (5 mol% Mo).