Assessing the thermal stability of UOW-10. (a) Thermogravimetric analysis (TGA) data collected from 50 to 1000 °C and (b) variable-temperature powder X-ray diffraction (VT-PXRD) of UOW-10 demonstrating the good thermal stability of the material and the formation of several phases upon structure collapse at temperatures greater than 410 °C. |