Figure 3
X-ray diffraction pattern of silver behenate on a (5 1 0) silicon wafer. The specimen was generated by spin-coating five drops of a silver behenate dispersion and rotating at ∼2000 r.p.m. The final silver behenate coating thickness was ∼3.2 µm. |