Figure 5
The elastic strain ∊22 measured in the vicinity of the crack tip for specimen CT1. The apparent vertical feature in the centre of the sample (at 6 mm) is due to missed data points when spectra were lost during a beam refill. |
|
Figure 5
The elastic strain ∊22 measured in the vicinity of the crack tip for specimen CT1. The apparent vertical feature in the centre of the sample (at 6 mm) is due to missed data points when spectra were lost during a beam refill. |