Figure 2
Typical lamellar cementite and ferrite with P–P 1 ORs in a 0.81C–Fe (wt%) specimen austenitized at 1103 K for 42 min and cooled at 2 K min−1. SEM secondary electron image. |
|
Figure 2
Typical lamellar cementite and ferrite with P–P 1 ORs in a 0.81C–Fe (wt%) specimen austenitized at 1103 K for 42 min and cooled at 2 K min−1. SEM secondary electron image. |