view article

Figure 4
Pore radius as a function of etching time for Makrofol N and LOFO polycarbonate membranes irradiated with 3 × 108 Xe ions cm−2 and etched in 5 M NaOH at 333 K; with (full symbols) and without (open symbols) UV treatment.