Figure 5
SAXS intensity as a function of scattering vector for LOFO samples (irradiated with 3 × 108 Xe ions cm−2) etched for 5 min (left) and for 8 min (right). In particular for small pores (left), UV-sensitized samples (red) exhibit much better resolved oscillations than untreated samples (blue). |