view article

Figure 4
4Gd-5Y alloy after T6 treatment: (a) HRTEM image of faceted β′ precipitates; (b) two-dimensional rough intensity map, at one of the positions at 6.24 keV (units on the axes are Å−1, auto-scaled intensity).