Structure factors of fluid Hg produced using SAXS and XRD at (a) T = 1773 K and ρ = 10.1 g cm−3 and (b) T = 1673 K and ρ = 9.62 g cm−3. The solid lines denote the experimental data and the dashed lines denote the obtained S(q).