Profiles of one-dimensional structure factor of SH300 along the stretching direction. The profiles are shifted vertically for clarity. Before elongation, a peak at q = 2 × 10−3 Å−1 is observed. On stretching the samples, the peak moves to a lower angle, and an additional peak appears at around 2.05 × 10−3 Å−1.