Figure 2
Mean-square radius of gyration determined from SAXS (filled symbols) and light scattering (unfilled symbols) measurements plotted against the degree of polymerization of main chain for the indicated polystyrene polymacromonomers in cyclohexane at 307.7 K (a) and in toluene at 298.2 K (SAXS) and 288.2 K (light scattering) (b). |