view article

Figure 9
(a) Raw detector image of a silver behenate sample taken at 60 Hz operation, SDD  =  3.9 m and a wavelength band of λ  =  3–6.7 Å. The data were collected for 107 min and binned along the TOF axis. The plot is on a logarithmic color scale. Light and dark stripes correspond to detector tubes in the front and back rows of the detector, respectively. Nine detector tubes (at x  =  63 and 136–143) were not functioning during this experiment. (b) The same data, binned along neutron momentum transfer axes Qx and Qy and plotted on a linear color scale.