The variations of the lattice spacing [a(\delta,z)] (evaluated from TiN 200 reflections) as a function of the coating depth and the angle δ indicate a relatively homogeneous stress state in the as-deposited coating (a) and pronounced residual stresses in the blasted coating surface (b).