Figure 8
Double-crystal topographs showing maps of the rocking curve COM and the FWHM for (a) the 300 µm-thick crystal mounted using nonperforated CVD diamond springs; (b) the 100 µm-thick crystal mounted using perforated CVD diamond springs; and (c) the 100 µm-thick crystal mounted using nonperforated CVD diamond springs. The units on the color bars are given in µrad. |
Open
access