view article

Figure 9
Double-crystal topographs (COM and FWHM) of the working crystal regions (∼5 × 2 mm) for (a) the 300 µm-thick crystal mounted using nonperforated CVD diamond springs; (b) the 100 µm-thick crystal mounted using perforated CVD diamond springs; and (c) the 100 µm-thick crystal mounted using nonperforated CVD diamond springs. The units on the color bars are given in µrad.