Normalized recorded rocking curves on a linear scale of the 444 reflections at 23.879 keV. Curve 1 (black) is measured as lapped; curve 2 (red) is measured after optical polishing (1 µm diamond grain); curves 3–5 (green, dark blue and light blue) are measured after 10, 20 and 30 min, respectively; curve 6 (purple) is measured after one MCP step between the optical polishing and the chemical etching(s).