Figure 2
XRD patterns of as-cast Mg–9.76 wt% Sn alloys aged for different times at 573 K after annealing at 823 K for 12 h. |
|
Figure 2
XRD patterns of as-cast Mg–9.76 wt% Sn alloys aged for different times at 573 K after annealing at 823 K for 12 h. |