Figure 3
(a) SEM secondary electron images of as-cast Mg–9.76 wt% Sn alloys aged (a) for 0 h and (b) at 573 K for 5 h after annealing at 823 K for 12 h. (c) Magnified SEM secondary electron image corresponding to the area marked by a white square in (b). |