Figure 2
Deviations from the average lattice parameter, expressed in the form Δa/a, for 48 measurements (top) and 24 pairs (bottom) for the Type 316L austenitic stainless steel. The average lattice parameter was 3.59500 Å and the standard deviations, expressed as a strain, were 84 and 42 × 10−6, respectively.