view article

Figure 2
Global sinograms of a 2%La–2%Mn–1.6%Na–3.1%W/SiO2 catalyst collected during an XRD-CT scan under ambient conditions using a 46 keV monochromatic pencil beam with a spot size of 2.5 × 2.5 µm. (Left) Raw data using the zigzag approach. (Right) The new global sinogram after sorting the values appropriately.