(a) Summed diffraction patterns for IXRD-CT scans 1 and 2. (b) A region of interest of the two diffraction patterns, showing the main diffraction peaks generated by the two Na2WO4 phases, Mn2O3, cristobalite, tridymite and quartz. |
|