view article

Figure 10
WAXS profile measured along the equatorial direction of the d-sPS cocrystal specimen after the simultaneous SANS/FTIR measurements on heating from 298 to 413 K. The reflections characteristic of the γ phase appear at 9.4 and 10.5°. The reflections at 6.9 and 8.3° are attributable to the and δ cocrystal components remaining in the specimen.