Measured (top), fitted (middle, R2 = 0.993) and differential (bottom) diffraction patterns of diamond data from POWGEN with 40 d⊥ slices and ΔDiv = 10. The color bar denotes the intensity as a percentage of the largest intensity peak in the experimental diffraction pattern. Reflections have been drawn broader than they really are to enhance the overall clarity. |