Comparison of stress components along the tensile load direction ([\sigma _{{33}}]) (distribution in the form of a histogram) for RVEs with 64, 216, 512, 1000, 3375, 4913, 8000 and 10 648 grains with the reference RVE (27 000 grains). The bin width of the histogram is 10 MPa.