Figure 9
ED diffraction pattern of the investigated ferritic steel sample, measured under ψ = 0°. The indices written in italics are diffraction lines of the weakly represented retained austenite phase. The slight asymmetry of the 110 ferrite line is due to the superposition with the 111 interference of the retained austenite. It was therefore excluded from further evaluation.