Figure 8
Quantification of the crystallographic signal quality within the experimental data set for the Al–Li–Mg–Ag alloy specimen (Gault et al., 2012a). (a) Thresholding via the image difference between the three individual signatures per ROI highlights again that the crystallographic signal is strongest in the pole regions. (b) The signature of the reference for the L12 crystal structure, here quantified with the atoms of the lithium substructure. (c) This reference is compared with an example ROI with signatures that were among the strongest of all detected. (d) The last results are compared with an example ROI with ill-defined signatures because of limited lithium counts. |