Figure 7
Specimen Ca/Si ratios of in situ XRD experiments. The calculations assume Ca/Si = 1.7 for C-(A)-S-H from Portland cement hydration and Ca/Si = 1.3 for additionally formed C-(A)-S-H (100–200 min), then Ca/Si = 1.3 alongside near-complete portlandite consumption (200–300 min), and eventually Ca/Si = 1.1 (300–600 min). |