Figure 3
EDX elemental analysis maps of an Fe–Ni crystal, showing the homogeneous elemental distribution of crystal 2B corresponding to the SEM spectrum in Fig. 1 (c). The images show the 2D signals for the primary Fe–Ni emission lines. |