view article

Figure 6
(a) XRR of the Co/TiOx/ML sample before and after reduction. For clarity, reflectivity curves have been displaced vertically with respect to each other. The continuous solid line represents the best fit to the experimental data. (b) XRF of Mo measured around BP1 and BP2 before and after reduction. (c) XRF of Ti measured around BP1 and BP2 before and after reduction. (d) Elemental distribution (for Ti and Mo) and δ profile (showing only the top bilayer of the multilayer) of the sample in the pristine and reduced states. The continuous solid line and dotted line represent the pristine and reduced states, respectively. A change in the total width of the Ti profile after reduction can be seen.