Figure 9
Diffraction images collected from an iron powder sample (but not from the same location) using (a) the same flat-panel detector with an exposure time of 170 s and (b) a photon-counting detector (Advacam ADVAPIX TPX3, 256 × 256 pixels and 55 µm pixel size, placed at an Lsd of 14 mm) with an exposure time of 1 s. The intensities are after normalization using a reference image collected under the same conditions but without the sample.