Phase-specific residual stresses (RS) created by welding of an HCT690T metal sheet, which was pre-deformed to a total strain of about 20% prior to bead-on-plate welding in the previous load direction. (a) The evolution of the phase-specific residual stresses of the ferrite phase depending on the distance to the weld seam center, determined in both the LD and the TD. Below the residual stresses, the associated evolution of the normalized mean integral breadth (IBn) of the X-ray interference lines is given. The Mathematical equation values determined in the LD are plotted versus Mathematical equation for distances of approximately (b) 8 mm and (c) 13 mm from the center of the weld seam.