view article

Figure 6
Fe 2p3/2 XAS spectra measured for (a) Fe/Ti and (b) Fe/Si at 450°C. (c) and (d) are the SEM images of Fe/Ti and Fe/Si, respectively, after the C2H2 exposure.

IUCrJ
Volume 1| Part 4| May 2014| Pages 221-227
ISSN: 2052-2525