Figure 13
Comparison of experimental Mn K-edge XANES spectra [from Guglieri et al. (2011)] of Ar-, Ar/N2- and Ar/O2-prepared Zn0.95Mn0.05O films and experimental data (PLD) reported by Pellicer-Porres et al. (2006) for Mn in ZnO wurtzite (w) structures. |