A part of the diffraction pattern of sample Ti0.53Al0.47N deposited at UB = −80 V, which illustrates the decomposition of the oversaturated fcc phase into Ti-rich fcc-(Ti,Al)N and Al-rich fcc-(Al,Ti)N. The measured intensities are plotted as open circles and the total calculated intensities as a solid line. The intensities diffracted by the dominant phase in the fcc-(Ti,Al)N sample are plotted as a thin solid line (red) and those diffracted by fcc-(Al,Ti)N as a dotted line (blue). Diffraction indices of the fcc phases are displayed at the top of the figure. The asterisks mark the diffraction lines from hex-WC.