Figure 9
Stress-free lattice parameters of fcc-(Ti,Al)N in samples Ti0.53Al0.47N (open symbols) and Ti0.44Al0.56N (filled symbols). The stress-free lattice parameters were converted to the aluminium content in Ti1−xAlxN using the Vegard-like dependence a0 = 4.2418 − 0.1432x (Å) from Rafaja, Wüstefeld et al. (2008BB30).