Left: Solid solution of BCNBP and DBBP. SPEM measurement at 325 Hz for a polished (b,c)-plane (results for two different crystals are shown). Right: SPEM measurement at 325 Hz for a polished (b,c)-plane of a pure BCNBP crystal. SPEM reveals two different bipolar states: left: ←→, right: →←.